1.888.282.3292

Alloy C276 Nickel Plate - UNS N10276


Hastelloy Alloy® C276 is an age-hardenable nickel-cobalt chromium-molybdenum alloy designed specifically to combine good age strength properties with excellent fabrication characteristics in the annealed condition.  The high molybdenum content provides resistance to localized corrosion. Low carbon minimizes carbide precipitation during welding. This alloy maintains very good corrosion resistance in a broad variety of chemcial process and aqueous environments. Alloy C276 exhibits excellent intermediate temperature tensile ductility, and is not normally subject to strain age cracking problems common for other gamma prime strengthened alloys. Alloy C276 is typically used for applications up to about 1650°F (900°C).

Standard Inventory Specifications 

  • UNS N10276
  • ASTM B 575
  • ASME SB 575
  • W.Nr 2.4819
  • NACE MR0175
  • NACE MR0103

Common Trade Names

  • Nicrofer 5716 hMoW (® ThyssenKrupp VDM)
  • Carpenter C-276 Alloy (® Carpenter Technology)
  • Inconel Alloy C-276 (® Special Metals)
  • Hastelloy C-276 (® Haynes International)

Common Applications of Alloy C-276 Nickel

  • Air pollution control (stack liners, ducts, dampers, scrubbers, stack-gas re-heaters, fans, and fan housings)
  • Chemical processing (heat exchangers, reaction vessels, evaporators, and transfer piping)
  • Pulp and paper production
  • Industrial and municipal waste treatment
  • Flue gas desulfurization system
  • Pickling baths
  • Aramide plastics production

Inventory Size Ranges

  • Plate : 0.1875" - 0.500"

All of our alloy C276 is ordered to specific decimal thickness. Please contact us for more details.

The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed.

Alloy C-276 Chemical Composition

Elements Percent By Weight
Chromium 14.5 - 16.5
Nickel Bal. Maximum
Manganese 1.0 Maximum
Silicon 0.08 Maximum
Vanadium 0.35 Maximum
Tungsten 3.5 - 4.5
Sulfur 0.03 Maximum
Carbon 0.01 Maximum
Iron 4.0 - 7.0
Phosphorus 0.04 Maximum
Molybdenum 15.0 - 17.0
Columbium 2.5 Maximum

 

 

Alloy C-276 Physical Properties

  • Density: 0.321 lb/in3
  • Melting Range: 2415-2500°F
   
Specific Heat at 70°F 0.102 Btu/lb °F
Elastic Modulus at 70°F 29.8 x 10 psi
Electrical Resistivity at 75°F 1.30 µΩ·m
Specific Gravity 8.90

 

Linear Coefficient of Thermal Expansion

Temperature °F 70 200 400 600 800 1000
10-6in/in/°F 5.9 6.4 7.5 8.7 9.8 11.0

 

Thermal Conductivity

Temperature°F 70 200 400 600 800 1000
Btu/h-ft-°F 5.9 6.4 7.5 8.7 9.8 11.0

 

Mechanical Properties and Yield Strength of Alloy C-276

Minimum Properties (ASTM B 575)  
Tensile Strength ksi [MPa] 10 [758]
Elongation % 40
Hardness [BHN] 100
Yield Strength (0.2% Offset) ksi [MPa] 41 [283]

 

Temperature, °F 70 200 400 600 800 1000
0.2 % Yield Strength (ksi) 60 55 50 46 42 39
Ultimate Tensile Strength 115 105 103 98 95 93
Elongation % 50 50 50 55 60 60

 